GOOD QUALITY RAW COTTON FIBERS ARE USED FOR THE MANUFACTURING OF THE ABOSRBENT COTTON WOOL IP SINKING TIME OF THE ABOVE NOT MORE THAN 8 SECONDS.
Other Specifications Download Specification | |
---|---|
Conformity To Indian Pharmacopieia Standard | IP 2007 VOL-2 |
Sterlity | Sterilized |
Sinking Time (Max) | 10 Sec |
Water Holding Capacity (Min) | 23 gm/ gm |
Thickness | 10 mm |
Width Of Roll | 38 mm |
Weight Of Roll | 500 Grams |
Packing Material | Plastic |
Availability Of Test Reports From Central Govt./NABL/IL AC Acredited Lab | Yes |
Test Report No | 551 |
Test Report Date | 21/03/2017 |
Name Of The Lab | Krishna Analytical |
Address Of The Lab | Mayapuri, Delhi |